Determining the three-dimensional morphology of γ′-particles in γ-γ′ superalloys

Citation

McElhaney, K. W., & Voorhees, P. W. (2000). Determining the three-dimensional morphology of γ′ -particles in γ-γ′ superalloys. Metallurgical and Materials Transactions A, 31 (5), 1333-42.

Abstract

We propose qualitative and quantitative methods for determining the three-dimensional morphology of second-phase particles in Ni-based superalloys in the late stages of coarsening. Qualitatively, we determine a way to identify the three-dimensional shape of a particle from its (111) cross section. Quantitatively, we derive a method that uses stereological analysis on a single (111) section to compute the average shape of a particle in three dimensions. For cases where the average shape does not necessarily reflect the particles’ true morphology, we derive another method based on sectioning probability to compute the shape of individual particles. We are also able to determine a particle’s orientation in three dimensions by examining its (111) cross section. The methods were tested by using computer-generated (111) sections of three-dimensional arrays of rectangular particles. We conclude that (111) sections can be used to provide an accurate calculation of the interfacial area per unit volume ( S V ) of the structure. Finally, we illustrate the efficacy of using (111) sections to determine particle morphology by examining (111) transmission electron microscopy (TEM) micrographs of particles undergoing splitting.


Read more from SRI

  • Banner and attendees at the IEEE Hard Tech Venture Summit

    Cultivating hard tech startups that scale

    IEEE’s Hard Tech Venture Summit convened innovators at SRI to refine strategies and build new networks.

  • Patient going into a MRI

    Bringing surgical tools inside the MRI

    Drawing on SRI’s unique innovation ecosystem, the startup Medical Devices Corner is seeking to improve cancer surgery by advancing MRI-safe teleoperation.

  • Christopher Mims and Susan Patrick

    PARC Forum: How to AI

    The Wall Street Journal tech columnist Christopher Mims and SRI Education’s Susan Patrick discuss how AI can strengthen human agency.